EN 10025-2 S235JR carbon steel chemical composition:
Thickness(mm) |
C |
Si |
Mn |
P |
S |
N |
Cu |
T≤16 |
0.17 |
... |
1.40 |
0.035 |
0.035 |
0.012 |
0.55 |
16<T≤40 |
0.17 |
||||||
40<T |
0.20 |
EN 10025-2 S235JR carbon steel mechanical property:
Thickness (mm) |
|||||||||
S235JR |
≤ 16 |
> 16 ≤ 40 |
> 40 ≤ 63 |
> 63 ≤ 80 |
> 80 ≤ 100 |
> 100 ≤ 150 |
> 150 ≤ 200 |
> 200 ≤ 250 |
> 250 |
Yield strength (≥Mpa) |
235 |
225 |
215 |
215 |
215 |
195 |
185 |
175 |
175 |
|
< 3 |
≥ 3 ≤ 100 |
> 100 ≤ 150 |
> 150 ≤ 250 |
> 250 |
||||
Tensile strength (Mpa) |
360-510 |
360-510 |
350-500 |
340-490 |
340-490 |
Equivalent grades of EN 10025-2 S235JR carbon steel:
EU |
USA |
Germany |
Japan |
France |
England |
European old |
Italy |
Belgium |
S235JR |
1015 |
RSt37-2 |
SM400A |
E24-2 |
40A |
Fe360B |
Fe360B |
AE235B |
EU |
Belgium |
China |
Sweden |
Russia |
Inter |
Portugal |
India |
Belgium |
S235JR |
AE235B |
Q235A |
1311 |
St2ps |
E235B |
IS226 |
AE235B |
EN 10025-2 S235JR carbon steel application: